Electrodes for corrosion and heat resistant CrNi and CrNiMo steels

 

Product
Standard
Weld Metal Analysis
Applications
Mechanical Properties
4829 Ti

AWS: E 309L – 16

DIN 8556:E 22 12 R 23

EN 1600:E 22 12 R 32

EN ISO 3581:E 22.12 L R 23

Recovery: 110%

Current: = (+) / ~

C:max. 0.05Cr: 21,0 – 23,0

Ni: 11,0 – 13,0

The electrode is suitable for joint welds of heat resistant CrNi-steels of the same kind or lower alloyed and for heat-resistant up to 1050 ºC.

It is important to know the possibility of surfacing on un-alloyed and low-alloyed (high temperature resistant) steels where 18-8 CrNi alloy is required in the first layer Suitable for following base materials:
1.2780, 1.4541, 1.4550, 1.4712, 1.4724, 1.4742, 1.4825, 1.4826, 1.4828

T: 520 – 560 N/mm²Y: 300 – 320 N/mm²E(1=5d): 33 – 38 %I: 65 – 75 Joule
4829 Mo Ti

AWS: E 309 Mo L – 16DIN 8556:E 23 12 3 R 23EN 1600:E 23 12 2 LR 32

EN ISO 3581:E 32.12.2 L 23

Recovery: 110%Current: = (+) / ~

C: <0,04Cr: 22,0 – 24,0

Ni: 11,0 – 13,0

Mo: 2,5 – 3,5

The electrode is suitable for joint welds of heat resistant CrNiMo-steels of the same kind or lower alloyed and for overlay welding on unalloyed steels if an 18-8-2 CrNiMo alloy is required in the first layer.It is important to know the possibility of welding unalloyed steels, low-alloyed steels or steels of difficult weldability with high alloyed steels or to each other.

T: 600 – 700 N/mm²

Y: 400 – 480 N/mm²

E(1=5d): 25 – 33 %

I: 50 – 70 Joule

4842 Ti

AWS: E 310 – 16DIN 8556:E 25 20 R 26EN 1600:E 25 20 R 12

EN ISO 3581:E 25.20 R 21Recovery: 100%Current: = (+) / ~

C:max. 0,1Cr: 24,0 – 26,0Ni: 19,0 – 21,0 Rutile-basic coated electrode for joint welds and overlays on scale-resistant and highly heat resistant CrNi-steels up to working temperatures of 1200 ºC. The weld deposit is resistant to gas of low sulphur and nitrogen. Well suited for welding of heat resistant Cr-, CrSi- and CrAl steels of ferritic-pearlitic structure in the field of furnace, pipeline and staple parts construction.Suitable for following base materials:
1.4713, 1.4762, 1.4710, 1.4841, 1.4845, 1.4849, 1.4848, 1.4846, 1.4828
T: 570 – 590 N/mm²Y: 320 – 340 N/mm²E(1=5d): 27 – 30 %I: 65 – 70 Joule